Epoxy 550

Make sure the surface is clean and free of any contaminants. After the floor has been profiled by diamond grinding or acid etching make sure the floor is thoroughly swept and vacuumed.
Mix 1 part A to 1 part B
Premix A before adding Part B, DO NOT MIX MORE MATERIAL THAT CAN BE APPLIED WITHIN 90 MINUTES at 77 Degree Fahrenheit. HIGHER TEMPERATURES REDUCE WORK TIME!!!!!
Measure the components carefully and mix for 2 minutes using a drill mixer being sure to scrape the bottom and sides of the mixing bucket. The material should be spread on using a flat trowel or squeegee. Wear spiked shoes to walk onto the wet material and back roll using a 1/2 inch roller nap. Use a brush around the edges. If concrete shadows appear to add additional products. Put color chips into wet material within 30 minutes of coating application.

Royal Metallic Epoxy Supply
501 Polyurethane

Mix only that amount of material that can be used in a 3 hour period at 77°F. Higher temperatures reduce work time. In hot weather, it is advisable to mix smaller batches. Premix Part A before adding part B. Mixing ratio is 2 parts A to 1 part B. Add part B slowly while mechanically agitating part A with a slow speed drill. Mix for 2 full minutes until completely mixed through. Thinning Material is normally applied as received but may be thinned with water up to 10% during application to keep a low viscosity. Any reduction water must be added after part A and B have been drill mixed. Application Recommendations Polyurethane 501 should be applied 200-350 sq. ft. per gallon by brush, roller or airless sprayer. Do not allow to puddle or accumulate in joint areas